Switching Inductor Design Calculator: Core, Gap, Wire and Losses

g Ae le N turns distributed gap
On the left a ferrite E core: the gap g is in the centre leg, the flux (dashed) loops through both outer legs and spreads out at the gap — that is fringing, which raises the inductance above the simple calculation. On the right a powder toroid: the gap is distributed among the grains of the material and cannot be seen.

Introduction

The inductor in a switching converter is almost always bought ready-made, and that is fine while the current is small. Above a few amps, or when you need a value no catalogue has, it pays to wind it yourself: a core, a bobbin, some enamelled wire. The trouble is that four parameters matter and they pull against each other — inductance, core saturation, copper loss and core loss — and in the end everything turns into a temperature.

The tool starts from the requirements — inductance, DC current, ripple, frequency — and tries every core it knows: gapped N87 ferrite on a bobbin, ferrite toroids, Micrometals iron-powder toroids and Magnetics powder toroids (MPP, Kool Mµ, High Flux). For each one it works out turns, gap and wire, then losses and temperature rise, and tells you which ones hold up. The candidate you like goes into the check, where you can change everything by hand and see inductance versus current, the losses harmonic by harmonic and the thermal balance.

Requirements can be taken from the switching converter calculator: design the converter there and the button below imports inductance, average current, ripple, frequency and duty cycle of the nominal point. Transformers and flyback coupled inductors are left out; they are in the ferrite transformer calculator.

QuantityFormulaWhat it decides
Minimum turns\( N = \dfrac{L\,I_{pk}}{B_{max}\,A_e} \)ferrite saturation
Inductance\( L = A_L\,N^2 \)gap, or powder permeability
Flux swing\( \Delta B = \dfrac{L\,\Delta I}{N\,A_e} \)core loss
Field in powder cores\( H = \dfrac{0{,}4\pi\,N\,I}{l_e} \)how much permeability is left under current

Card 1 — Requirements

Design rules
Core families to try

The first seven fields are the converter: the inductance you need, the average current through it, the peak-to-peak ripple, the frequency and the duty cycle, which sets the shape of the triangle — rising for D·T and falling for the rest of the period. The shape matters, because core loss and high-frequency copper loss depend on how steep each ramp is.

The design rules are the bench ones. A J of 4–6 A/mm² is the usual value for an inductor in still air; fill is counted with the enamelled wire, and a hand-wound toroid does not go beyond 40–45 %. Ferrite Bmax stays below the hot saturation, which for N87 at 100 °C is 390 mT. The minimum gap keeps you independent of ferrite tolerance: below a tenth of a millimetre the material decides the inductance more than the gap does.

Minimum residual µ applies to powders: it is the fraction of initial permeability left at peak current. 50 % is a common compromise; lower than that the inductance changes too much between no load and full load.

Card 2 — Candidate cores

CoreNGapConductorFillCopperCoreΔTVerdict

Each family has its own rule. With bobbin ferrite you start from the minimum turns that keep peak B below Bmax, compute the gap that gives the inductance, and add a few turns until the gap exceeds the minimum and total losses stop falling: more turns mean less flux swing and less core loss, but more copper. Next to the custom gap the tool shows the catalogue gap you can buy already ground, with the turns it needs.

Powders have no gap: turns are added until the inductance under DC current reaches the required value. Each extra turn also raises the field, and permeability drops: if the core is too small you reach a point where more turns no longer help, and the tool says so. Ungapped ferrite toroids are in the list for completeness, and almost always saturate: they suit common-mode filters, not an inductor carrying DC.

The wire is chosen from the current density. With “best of the three” the tool tries a single wire, parallel strands no thicker than 2δ and litz with strands no thicker than δ, and keeps the one with the least loss that fits the window; within a few percent the simplest wins. Rows are ordered by verdict and then by core volume.

Card 3 — Checking an inductor

Here the inductor is yours: core, turns, gap and wire can be changed by hand, and the rest of the page follows. The graph is inductance versus current. For a powder it is a slowly falling curve, and you want it still above the orange line at the DC current; for a gapped ferrite it is flat until B reaches saturation, and there it collapses at once — the red segment is only indicative, because beyond Bs no simple model holds.

Ferrite saturation depends on temperature: N87 goes from 490 mT at 25 °C to 390 mT at 100 °C, and the tool uses the value at the temperature it computes for the inductor. An inductor that is fine when cold can saturate after half an hour of running.

Gap and fringing

Core and gap are two reluctances in series. The core one comes from the datasheet’s ungapped AL, which already contains the real material permeability and the joints between the two halves:

\( A_L(g) = F \cdot \left( \dfrac{1}{A_{L0}} + \dfrac{g}{\mu_0 A_e} \right)^{-1} \)

F is the fringing factor: at the gap the flux spreads outside the leg, the useful cross-section grows and the inductance is higher than the simple calculation. It is not estimated with a formula: it is derived from the gapped AL values TDK prints for each core, comparing them with the no-fringing calculation, and interpolated between one gap and the next. For the ETD 34 it is 1.13 at 0.5 mm and 1.67 at 2.5 mm. Where there is no table, F = 1 and the tool flags it.

The catalogue gap s is in the centre leg only. If you have no ground cores you can put an insulating spacer of thickness s/2 between the two halves: the flux crosses two gaps, the centre-leg one and the outer-leg one, which in E and ETD cores together have about the same cross-section, and the result is close. Fringing on the outer legs differs, though, and the inductance has to be measured.

Powder permeability under DC current

In powders permeability drops with the DC field following the manufacturers’ DC-bias curves, which Micrometals and Magnetics publish in the same form:

\( \%\mu = \dfrac{1}{a + b\,H^{c}} \qquad H = \dfrac{0.4\pi\,N\,I}{l_e}\ \text{[Oe, } l_e \text{ in cm]} \)

Magnetics curves are typical values; the individual core datasheets guarantee a minimum instead, for example 80 % of permeability at 39 Oe for Kool Mµ 60µ, where the curve gives 84 %. Peak B in a powder is obtained by integrating permeability along the field, from zero to the peak value.

Card 4 — High-frequency copper, losses and temperature

HarmonicFrequencyRMS currentΔFRLoss

The inductor current is DC with a triangle on top. The DC heats the copper through its Rdc; the triangle breaks down into its harmonics, and each one sees a higher resistance, because at high frequency current crowds to the skin of the wire and neighbouring layers steal it from one another. The tool computes the factor FR = Rac/Rdc for each harmonic with Dowell’s model and adds up the losses.

\( I_n = \dfrac{\Delta I\,\sin(n\pi D)}{n^2\pi^2 D(1-D)} \qquad \Delta = \left(\dfrac{\pi}{4}\right)^{3/4} \dfrac{d}{\delta_n}\sqrt{\eta} \qquad \delta_n = \sqrt{\dfrac{\rho}{\pi\,n f\,\mu_0}} \)

\( F_R = \Delta \left[ \dfrac{\sinh 2\Delta + \sin 2\Delta}{\cosh 2\Delta – \cos 2\Delta} + \dfrac{2(m^2-1)}{3}\,\dfrac{\sinh\Delta – \sin\Delta}{\cosh\Delta + \cos\Delta} \right] \)

The first term is skin effect, the second proximity effect, which grows with the square of the number of layers m: this is why ten thin strands in parallel on five layers can run hotter than one thick wire on one layer. In litz the strands are twisted and each one passes through every position: the tool treats it as √n strand layers for each layer of bundle.

Core loss with a triangle wave

Manufacturers give core loss with a sine wave. With a converter’s triangle, at equal flux swing, the loss changes with the duty cycle: a short steep ramp does more harm than two equal ramps. The tool uses the improved generalised Steinmetz equation (iGSE, Venkatachalam et al., 2002), which carries the sine data over to the real waveform with a factor that depends only on D and the frequency exponent α:

\( P_v = P_{v,\sin}\!\left(f, \tfrac{\Delta B}{2}\right) \cdot \dfrac{2^{\alpha}\left[D^{1-\alpha} + (1-D)^{1-\alpha}\right]}{(2\pi)^{\alpha-1}\displaystyle\int_0^{2\pi} |\cos\theta|^{\alpha}\,d\theta} \)

For N87 the sine data come from a Steinmetz fit I made on the four loss points TDK prints at 100 °C, within 5 %; for Magnetics powders from the published curve fits; for Micrometals from its four-coefficient formula, from which the tool computes local α and β. The box under the table compares the model with the maximum loss the datasheet guarantees at its test point. The superimposed DC raises ferrite loss somewhat, and none of the models accounts for it.

How temperature is estimated

For toroids the rule is Magnetics’: \( \Delta T = (P\,[\text{mW}] / A\,[\text{cm}^2])^{0.833} \), with A the surface of the wound inductor, which Magnetics prints unwound and at 40 % fill. For the other toroids the surface is computed from the dimensions with the same increase with fill, calibrated on the Magnetics data.

For bobbin cores the empirical rule \( R_{th} \approx 53 / \sqrt{V_e\,[\text{cm}^3]} \) °C/W is used, in still air. Both give an order of magnitude: an inductor closed in a box, near a heatsink or lying on a copper plane changes by several degrees. Copper resistance is recomputed at the temperature found, and the calculation repeats until it settles.

The mean turn length of Magnetics toroids is the printed one, as a function of fill; for the other toroids it is computed as \( 2w + 2h + 4.5\,t \), with w and h the sides of the cross-section and t the winding thickness on the inner diameter — on the three Magnetics toroids the formula is within 1 % of the printed values. For bobbins it is the TDK datasheet lN.

Preloaded cores and materials, sources

CoreMaterialAe (mm²)le (mm)Ve (cm³)AL (nH)Window (mm²)Catalogue gaps (mm → nH)

The core name opens the datasheet in a new window. The window is the bobbin winding area (AN) for TDK cores and the hole area, with coating, for toroids. N87 losses come from the TDK material datasheet (June 2025), powder losses from the Micrometals formulas (revision 20190524) and the Magnetics material curve fits. Two values are not the manufacturer’s and are declared as such: the N87 Steinmetz coefficients, derived with a fit, and the usable bobbin width when you do not enter it.