A watt of electrical input at the LED, a watt of UV radiation and a given number of photons are three different conditions. I use two commercially available emitters to work out which quantity to hold fixed when comparing photocatalysis at two wavelengths.

In the first article I compared the UV bands used in photocatalysis. Here I track the photons from the LED to the TiO₂ plane. The datasheets give the emitted power. I use an illustrative model for the window, geometry and illuminated area, then describe how I would test it on the bench.

Two LEDs at documented operating points

For UVA I use the Seoul Viosys CUN66A1B, a 365 nm class LED. Table 1 of its datasheet gives a 367 nm peak at 500 mA, so I use 367 nm in the calculations. For UVC I use the Violumas VS5252C48L6-265-V2. Its typical radiant flux is 130 mW at 700 mA. The datasheets specify temperature at different reference points. Both operating points should be checked in the actual assembly with the LED at thermal equilibrium. [1] [2]

Manufacturer data at the respective characterization points
QuantitySeoul Viosys CUN66A1BViolumas VS5252C48L6-265-V2
Peak wavelength367 nm, 365 nm class265 nm typical
Forward current500 mA700 mA
Forward voltage3.7 V6.2 V typical
Emitted radiant flux1.00 W0.130 W typical
Spectral full width at half maximum9 nm13 nm typical
Specified emission angle120°60°
Reference temperatureSolder point at 25 °CAmbient at 25 °C

Current times voltage gives 1.85 W of electrical input for the Seoul LED and 4.34 W for the Violumas. The ratios of emitted radiant power to electrical input at the terminals are about 54% and 3.0%. A first-order heat balance leaves about 0.85 W and 4.21 W to dissipate at the devices. Driver and cooling loads are additional. Thermal design depends on the full junction-to-ambient thermal resistance and operating conditions, as well as package data. [1] [2]

From the LED to the catalyst plane

I consider an immobilized catalyst on a 10 cm² plane. The model captures 40% of the emitted power in both setups. The window transmits 90% at 367 nm and 85% at 265 nm. All three coefficients are assumptions. Using the same 40% isolates the other factors. With different emission angles, collection can vary substantially even with the same mounting geometry. The actual window requires transmission data for the appropriate material, thickness and coating. I assume negligible attenuation by the medium after the window. [3]

Pinc ≈ Pem × fgeom × Twin
Eavg = Pinc / A

Here Pinc is the radiant power incident on the plane, fgeom is the collected fraction, Twin is effective window transmittance, and Eavg is mean irradiance. I divide the incident power by the energy of one photon to count photons per second, then divide by Avogadro’s constant to get a molar flow. [4]

Eγ = hc / λ
ṅγ ≈ Pinc λ / (NAhc)

With power in watts and wavelength in metres, the result is in mol/s. Multiply by 3.6 × 10⁶ to obtain mmol/h. The peak wavelength is a narrowband approximation. With a measured spectrum at the plane, I would multiply the power in each spectral interval by λ/(NAhc) and sum the contributions.

Bars show emitted, captured and incident power. The catalyst plane receives 360 and 44.2 mW.
Figure 1. Radiant power from the LED to the plane. The first group comes from the datasheets. The other two apply the assumed collection and transmission coefficients.
Calculated at the datasheet operating points under the stated assumptions
Quantity367 nm265 nm
Emitted photons11.04 mmol/h1.04 mmol/h
Radiant power at the plane360 mW44.2 mW
Mean irradiance over 10 cm²36.0 mW/cm²4.42 mW/cm²
Incident photon flux3.98 mmol/h0.352 mmol/h
Mean photon flux density1,104 µmol/(m²·s)97.9 µmol/(m²·s)

In this example, the plane receives about 11.3 times as many photons from the Seoul LED as from the Violumas at their respective datasheet operating points. The ratio depends on the devices and assumptions. How many photons the TiO₂ absorbs also depends on reflection, transmission through the layer, and absorption by the support or the medium.

Three comparisons answer three questions

1. Equal electrical input

As a first energy comparison, I divide the photon flux at the plane by the electrical input at each LED’s datasheet operating point. I obtain 2.15 mmol/h per watt at 367 nm and 0.0812 mmol/h per watt at 265 nm, a ratio of about 26.5. To compare two sources at the same actual consumption, I would measure upstream of the drivers and include auxiliary loads. Flux need not scale linearly with current.

2. Equal incident radiant power

At 30 mW at the plane in both cases, the flux is 0.331 mmol/h at 367 nm and 0.239 mmol/h at 265 nm. The ratio is 367/265, about 1.38. For the same radiant energy per second, more photons arrive at the longer wavelength because each carries less energy. If I match power at the LED output, I still need to measure how much reaches the plane.

3. Equal incident photon flux

If I use 30.0 mW incident at 265 nm as the reference, I set 21.7 mW incident at 367 nm. Both give about 0.239 mmol/h at the plane, or a mean of about 66.5 µmol/(m²·s) over 10 cm². I would adjust the sources using radiometric measurements. At equal incident flux, the catalyst can still absorb a different fraction at each wavelength.

The 367-to-265 nm ratio is 26.46 per electrical watt, 1.38 at equal radiant power and 1 at equal photon flux.
Figure 2. Ratio of incident photon fluxes. The first value uses the model and datasheet operating points. The second depends on the wavelengths. In the third comparison, photon flux is the controlled quantity.

I would start the reactor comparison at equal incident photon flux. I would run a separate energy comparison and record total consumption. In an actual reactor I would also measure the spatial distribution, since the same total can come from a concentrated beam or a more uniform field.

From calculations to bench measurements

  1. Stabilize the sources. Use a constant-current driver for each LED and record current, voltage and temperature near the package using the same procedure. Measure power upstream of the drivers for the energy comparison.
  2. Measure at the catalyst plane. Use a radiometer or spectroradiometer calibrated in both bands. Keep the window and optical path representative of the reactor, then measure irradiance on a grid at the plane. An area-weighted sum estimates total power. Measurements outside the liquid require a verified correction and its uncertainty. Detector spectral response can affect comparisons across UV bands. [5]
  3. Repeat at equal photon dose. At constant flux, dose is flux multiplied by time. Record repeated readings, thermal stability, calibration uncertainty and spatial variability. An actinometer suited to the band and geometry can provide an independent check in the measurement volume. Estimating TiO₂ absorption requires a measurement on the catalytic system. [6]

UV safety. Place the sensor before switching on and make measurements in a shielded, interlocked enclosure. Direct UVC exposure can cause acute eye or skin injury. Directive 2006/25/EC covers occupational exposure to artificial optical radiation in the EU. [7] [8]

An irradiance map for each source gives me a reproducible starting point. The next step is to compare the chemical transformation with and without TiO₂ to measure the effect of UV in the absence of the catalyst.

Sources and data

  1. Seoul Viosys, CUN66A1B, datasheet Rev. 15.1. Table 1, emission spectrum, current and temperature dependence, and angular distribution.
  2. Violumas, VS5252C48L6-265-V2, datasheet Rev. 010926. Electro-optical table, spectrum and angular distribution.
  3. Thorlabs, UV fused-silica windows. Transmission curves for different coatings.
  4. BIPM, International System of Units. Exact values of h, c and NA.
  5. NIST, Standardization of UV LED measurements. Spectral response and calibration.
  6. Kuhn, Braslavsky and Schmidt, Chemical actinometry. IUPAC, Pure and Applied Chemistry 76, 2105–2146.
  7. FDA, Ultraviolet (UV) Radiation. Effects of UV-C on eyes and skin.
  8. Directive 2006/25/EC on artificial optical radiation

The plots are original calculations based on the datasheets and the numerical model described here.